The natural extension ratio is the main caracteristic of the plastic failure zone

https://doi.org/10.35164/0554-2901-2016-7-8-61-63

Abstract

The method of determination of the natural extension ratio in plastic failure zone after hydraulic pressure test was develop. The volume of natural extension ratiodeterment in uniaxial and double axial loading conditions is the same. The ratio between surface and volume of the test pieces was analyzed for different kinds of polyethylene.It shows that for the different kinds of polyethylenethe natural extension ratiocan bevery different, up to two times.

About the Authors

В. Колбая
ООО «Климовский трубный завод»
Russian Federation


В. Коврига
ООО «Группа ПОЛИМЕРТЕПЛО»
Russian Federation


References

1. Э.М. Айзенштейн. Разработка процессов производства полиэфирных волокон, основанных на принципах физической и химической модификации полиэтилентерефталата. Диссертация на соискание учёной степени д.т.н. Калинин 1983. С.68.

2. А.Л. Волынский и Н.Ф. Бакеев. Роль поверхностных явлений в структурно-механическом поведении твёрдых полимеров. - М.: ФИЗМАТЛИТ, 2014.-356с.

3. СТО 73011750-012-2014. Пластмассы. Метод определения параметров зоны пластического разрушения полимерных труб.


Review

For citations:


 ,   The natural extension ratio is the main caracteristic of the plastic failure zone. Plasticheskie massy. 2016;(7-8):61-63. (In Russ.) https://doi.org/10.35164/0554-2901-2016-7-8-61-63

Views: 252


Creative Commons License
This work is licensed under a Creative Commons Attribution 4.0 License.


ISSN 0554-2901 (Print)