Obtaining of nitrogen-containing monoalkyl (C8-C12)phenolformaldehyde oligomers, grafted with esters of oleic acid and aliphatic alcohols
https://doi.org/10.35164/0554-2901-2017-9-10-17-19
Abstract
About the Authors
M. N. AmiraslanovaRussian Federation
A. M. Mustafaev
Russian Federation
R. A. Rustamov
Russian Federation
Y. G. Abdullaev
Russian Federation
P. E. Isaeva
Russian Federation
F. A. Mamedzade
Russian Federation
S. F. Akhmedbekova
Russian Federation
A. P. Alieva
Russian Federation
References
1. Li Jinhui, Jia Li-chun, Du Chao-jun. Modification of phenol-formaldehyde resins for aqueous coating systems // Plat. and Finish, 2005, V.27, № 1. P. 35-37
2. Лифшиц М.Л., Пшиялковский В.И.Лакокрасочные материалы. Химия: Москва, 1982, с. 63-68
3. Yuan Xin-hua, Shao Mei-xiu, Chen Min et al. Preparation and heat endurance of phenolic resin modified with linseed oil // Jiangsu Univ. Natur. Sci., 2006, V.27, №3, p. 234-236
4. Yuan Xin-hua, Chen Min, Shao Mei-xiu et al. Investigation of phenolic resin modified with linseed oil and used for producing of the friction material //Polym. Mater. Sci. Technol. Eng., 2006, V.22, №6, p. 181-183,187
5. Liu Tao, Zeng Liming. The development of research in the field of мodified phenolic resins used for the production of friction materials // Plast. Sci. and Technol., 2008, V.36, №12, p.84-89
6. Амирасланова М.Н., Мустафаев А.М., Рустамов Р.А., Ибрагимова М.Дж., Исаева П.Э., Алиева Ш.Р., Ахмедбекова С.Ф. Азотсодержащие моноалкил(С8-С12)ФФО, привитые с природными триглицеридами, в качестве защитных покрытий // Положительное решение № а 20140051 (24.06.2014).
Review
For citations:
Amiraslanova M.N., Mustafaev A.M., Rustamov R.A., Abdullaev Y.G., Isaeva P.E., Mamedzade F.A., Akhmedbekova S.F., Alieva A.P. Obtaining of nitrogen-containing monoalkyl (C8-C12)phenolformaldehyde oligomers, grafted with esters of oleic acid and aliphatic alcohols. Plasticheskie massy. 2017;(9-10):17-19. (In Russ.) https://doi.org/10.35164/0554-2901-2017-9-10-17-19